Determination of Susceptibility To Intergranular Corrosion of Uns 31803 Type Duplex Stainless Steel by Electrochemical Reactivation Method
dc.authorid | Doruk, Mustafa Çağrı/0009-0000-8238-2521 | |
dc.authorscopusid | 36805393400 | |
dc.authorscopusid | 6603467702 | |
dc.authorscopusid | 6603219850 | |
dc.authorwosid | Doruk, Mustafa Çağrı/KSL-8951-2024 | |
dc.contributor.author | Arikan, Mehmet Emin | |
dc.contributor.author | Arikan, Rafet | |
dc.contributor.author | Doruk, Mustafa | |
dc.contributor.other | Department of Mechanical Engineering | |
dc.date.accessioned | 2024-07-05T15:10:10Z | |
dc.date.available | 2024-07-05T15:10:10Z | |
dc.date.issued | 2012 | |
dc.department | Atılım University | en_US |
dc.department-temp | [Arikan, Mehmet Emin; Doruk, Mustafa] METU, Dept Met & Mat Engn, TR-06531 Ankara, Turkey; [Arikan, Rafet] Atilim Univ, Dept Mech Engn, TR-06836 Ankara, Turkey | en_US |
dc.description | Doruk, Mustafa Çağrı/0009-0000-8238-2521 | en_US |
dc.description.abstract | Specimens taken from a hot-rolled cylindrical duplex stainless steel (DSS) bar with 22% Cr grade were solution annealed at 1050 9 degrees C and then aged at 725. C from 100 to 31622 min for sensitization treatment. Double loop electrochemical potentiodynamic reactivation and standard weight loss immersion acid tests were conducted. The solution-annealed samples were found unsensitized. Those samples aged for 100 and 316 min were less sensitized whereas samples aged for 1000 min and especially those aged for 3162, 10000, and 31622 min were heavily sensitized. The degree of sensitization (DOS) can be attributed to higher contribution of chromium-and molybdenum-depleted areas resulting from intermetallic phases. | en_US |
dc.identifier.citationcount | 4 | |
dc.identifier.doi | 10.1155/2012/651829 | |
dc.identifier.issn | 1687-9325 | |
dc.identifier.issn | 1687-9333 | |
dc.identifier.scopus | 2-s2.0-84873864484 | |
dc.identifier.scopusquality | Q2 | |
dc.identifier.uri | https://doi.org/10.1155/2012/651829 | |
dc.identifier.uri | https://hdl.handle.net/20.500.14411/1277 | |
dc.identifier.volume | 2012 | en_US |
dc.identifier.wos | WOS:000215224400032 | |
dc.institutionauthor | Arıkan, Rafet | |
dc.language.iso | en | en_US |
dc.publisher | Hindawi Ltd | en_US |
dc.relation.publicationcategory | Makale - Uluslararası Hakemli Dergi - Kurum Öğretim Elemanı | en_US |
dc.rights | info:eu-repo/semantics/openAccess | en_US |
dc.scopus.citedbyCount | 6 | |
dc.subject | [No Keyword Available] | en_US |
dc.title | Determination of Susceptibility To Intergranular Corrosion of Uns 31803 Type Duplex Stainless Steel by Electrochemical Reactivation Method | en_US |
dc.type | Article | en_US |
dc.wos.citedbyCount | 4 | |
dspace.entity.type | Publication | |
relation.isAuthorOfPublication | 1795165c-1e5b-4512-a9be-3003d12d7202 | |
relation.isAuthorOfPublication.latestForDiscovery | 1795165c-1e5b-4512-a9be-3003d12d7202 | |
relation.isOrgUnitOfPublication | f77120c2-230c-4f07-9aae-94376b6c4cbb | |
relation.isOrgUnitOfPublication.latestForDiscovery | f77120c2-230c-4f07-9aae-94376b6c4cbb |