In this study, the microstructural formation and static/dynamic compression behaviour of recycled Ni-Al-Cu matrix hybrid composites reinforced with silicon whiskers and alumina (Al2O3) fibres will be studied. It is intended to be an alternative to traditional alloys/composites used in the aeronautical industry. These composites generally are produced using by combined “sintering + forging” processes. The static and dynamic properties will be evaluated in detail, considering the relevant scanning electron microscopy (SEM) microstructures (including the distribution of reinforcement elements). © 2023, The Society for Experimental Mechanics, Inc.
Açıklama
Anahtar kelimeler
Recycled composites, SEM, SiCws, Static and dynamic tests, γ-Al<sub>2</sub>O<sub>3</sub>, [CHIM.MATE] Chemical Sciences/Material chemistry, [PHYS.MECA.MEMA] Physics [physics]/Mechanics [physics]/Mechanics of materials [physics.class-ph], [SPI.MAT] Engineering Sciences [physics]/Materials
Bilim Dalları
0205 materials engineering, 02 engineering and technology
Alıntı
WoS Q
Scopus Q
Cilt
Sayı
Başlangıç Sayfası
29
Bitiş Sayfası
35
Doaj Url
Koleksiyonlar
Yükleniyor...